Study on Comprehensive Recovery of Vanadium, Titanium and Phosphorus from Chengde Super-depleted Vanadium Titanium Magnetite Mine

<

The project is a science and technology project initiated by the Ministry of Land and Resources of Hebei Province. It was completed by the Laboratory of Hebei Province Geology and Minerals Center. In January 2008, it was approved by the Hebei Provincial Department of Land and Resources.

Chengde Vanadium and Titanium ultra-lean magnetic iron ore is the famous temple of a sub-type vanadium-titanium magnetite minerals, as well as success in recent years to develop new mineral utilization in Hebei Province. In addition to iron, ultra-depleted vanadium-titanium magnetite is accompanied by minerals such as vanadium (V), titanium (Ti) and phosphorus (P). However, in the development and utilization of mines, most mining enterprises have not comprehensively recycled and associated minerals such as vanadium, titanium and phosphorus. Only a few mining enterprises have comprehensively recycled and utilized resources such as titanium and phosphorus, and the comprehensive recycling rate is low. Recycled resources such as vanadium, titanium and phosphorus are difficult to recycle. In order to promote the comprehensive recycling of resources, in 2007, the Planning and Design Institute of Chengde City Land and Resources Bureau cooperated with the Laboratory of Hebei Province Geology and Minerals Center to carry out and complete the vanadium and titanium of ultra-depleted vanadium-titanium magnetite (tailings) in Chengde City, Hebei Province. Research on the comprehensive recycling of phosphorus and other elements.

On the basis of the comprehensive recovery process of the associated elements of the “Da-Miao” vanadium-titanium magnetite, the research work first uses optical microscopy, scanning electron microscopy, spectral analysis, chemical analysis, phase analysis and electron probe analysis. Comprehensive analysis and analysis of ore material composition, ore properties and ore processing technology; selected 8 representative mining areas, for the nature of ore, using the difference in physicochemical properties such as mineral magnetization coefficient, specific gravity and floatability, using magnetic separation, floating and reselection methods such election, magnetite, ilmenite, apatite and optional mineral comparative tests were summarized recommend the single integrated iron and selected from the group selected from phosphorus, titanium election process, i.e., "coarse separator , coarse concentrate re-magnetization - shaker - strong magnetic separation titanium process" or "original - magnetic separation - flotation - titanium recovery process". The magnetite in the ore can be recovered by the weak magnetic method; vanadium has no separate minerals, but is present in the vanadium-titanium magnetite in the form of isomorphism, and is recovered by smelting; the single crystal of ilmenite can be obtained by strong magnetic method or heavy The magnetic flotation combined process is recycled; the apatite is floatable and can be directly recovered from the iron ore tailings by flotation. The process provides reference and reference for the beneficiation process to improve the comprehensive utilization level of titanium, phosphorus and other elements in the ultra-lean vanadium-titanium magnetite resources. At the same time, based on the current iron ore and phosphate geological exploration specifications, the ore is proposed based on the analogy analysis. The lowest industrial indicators for the comprehensive utilization of intermediate components such as titanium and phosphorus are recommended.

Through research, optional industrial experiments and mine production, it is shown that the selection of titanium and phosphorus-selecting technology from tailings is feasible and economically reasonable. The average grades of titanium and phosphorus are all around 2%, and the grade of phosphate concentrate can reach 33%. Above, the grade of titanium concentrate is over 46%.

In addition, the project also studied the impact of tailings on the geological environment and the use of tailings, and proposed the use of the project.

The project is a science and technology project initiated by the Ministry of Land and Resources of Hebei Province. It was completed by the Laboratory of Hebei Province Geology and Minerals Center. In January 2008, it was approved by the Hebei Provincial Department of Land and Resources.

Chengde super-depleted vanadium-titanium magnetite is a sub-mineral of the famous Damiao-type vanadium-titanium magnetite in China, and it is also a new mineral that has been successfully developed and utilized in Hebei Province in recent years. In addition to iron, ultra-depleted vanadium-titanium magnetite is accompanied by minerals such as vanadium (V), titanium (Ti) and phosphorus (P). However, in the development and utilization of mines, most mining enterprises have not comprehensively recycled and associated minerals such as vanadium, titanium and phosphorus. Only a few mining enterprises have comprehensively recycled and utilized resources such as titanium and phosphorus, and the comprehensive recycling rate is low. Recycled resources such as vanadium, titanium and phosphorus are difficult to recycle. In order to promote the comprehensive recycling of resources, in 2007, the Planning and Design Institute of Chengde City Land and Resources Bureau cooperated with the Laboratory of Hebei Province Geology and Minerals Center to carry out and complete the vanadium and titanium of ultra-depleted vanadium-titanium magnetite (tailings) in Chengde City, Hebei Province. Research on the comprehensive recycling of phosphorus and other elements.

On the basis of the comprehensive recovery process of the associated elements of the “Da-Miao” vanadium-titanium magnetite, the research work first uses optical microscopy, scanning electron microscopy, spectral analysis, chemical analysis, phase analysis and electron probe analysis. Comprehensive analysis and analysis of ore material composition, ore properties and ore processing technology; selected 8 representative mining areas, for the nature of ore, using the difference in physicochemical properties such as mineral magnetization coefficient, specific gravity and floatability, using magnetic separation, floating Selection and re-election methods, the ore selection test of magnetite, apatite and ilmenite was compared, and a single iron selection and comprehensive phosphorus selection and titanium selection process were recommended, namely “rough grinding magnetic separation”. , coarse concentrate re-magnetization - shaker - strong magnetic separation titanium process" or "original - magnetic separation - flotation - titanium recovery process". The magnetite in the ore can be recovered by the weak magnetic method; vanadium has no separate minerals, but is present in the vanadium-titanium magnetite in the form of isomorphism, and is recovered by smelting; the single crystal of ilmenite can be obtained by strong magnetic method or heavy The magnetic flotation combined process is recycled; the apatite is floatable and can be directly recovered from the iron ore tailings by flotation. The process provides reference and reference for the beneficiation process to improve the comprehensive utilization level of titanium, phosphorus and other elements in the ultra-lean vanadium-titanium magnetite resources. At the same time, based on the current iron ore and phosphate geological exploration specifications, the ore is proposed based on the analogy analysis. The lowest industrial indicators for the comprehensive utilization of intermediate components such as titanium and phosphorus are recommended.

Through research, optional industrial experiments and mine production, it is shown that the selection of titanium and phosphorus-selecting technology from tailings is feasible and economically reasonable. The average grades of titanium and phosphorus are all around 2%, and the grade of phosphate concentrate can reach 33%. Above, the grade of titanium concentrate is over 46%.

In addition, the project also studied the impact of tailings on the geological environment and the use of tailings, and proposed the use of the project.

EDAWELD Co., Ltd. professional production Plasma Consumables Compatible for Komatsu. We have Plasma Cutting Nozzle,electrode and shield compatible for Twister 30KW. Komatsu is very famous Japan brand, Japanese Plasma Consumables. Our copy Komatsu Plasma Consumables are made by imported high-quality copper and use superb CNC technology. So they got bright surface and cutting speed, less wear and tear, as compared with the original parts, we can reach 90%. But our low prices, it is worth buying.

Plasma Consumables Compatible for Komatsu

Plasma Consumables Compatible for Komatsu,Twister 30KW Nozzle,Twister 30KW Electrode,969-95-24190 Nozzle,969-95-24910 Electrode

EDAWELD COMPANY LIMITED , http://www.jsedaweld.com